Thermal Stability of New Polyamide Containing 1-Phenethyl-4-Piperidone Moiety in the Main Chain
الكلمات المفتاحية:
Polyamide، 1-Phenethyl-4-Piperidone، Thermal stability.الملخص
A new polyamide based on pyridine moiety was synthesized from 3,5-bis(4-aminobenzylidene) -1-Phenethyl-4-Piperidone (II) by reaction with 2,6-Pyridinedicarbonyl chloride using solution polycondensation technique. The polymer was obtained has yellow color and had inherent viscosity 0.86 dL/g. The solubility of polyamide was insoluble in common organic solvents but dissolved completely in concentrated H2SO4. The thermal properties of the polyamide was evaluated and correlated to their structural units by TGA and DSC measurements. Electrical conductivity in the range of 2.4 X 10-11 Ω-1 cm-1.at room temperature.
المراجع
1.Seymour RB and Carraher CE. Polymer Chemistry, an Introduction.Marcel Dekker: New York, 2000; 263.
2.Cassidy PE. Thermally Stable Polymers. Marcel Dekker: New York,1980; 71.
3.Peckham J, Gomez-Elipe P and Manners I. Metallocene based polymers. In Metallocenes; Synthesis, Reactivity and Applications, Vol. 2, Togni A and Halterman RL (eds). Wiley-VCH: New York,1998;723.
4.Fery-Forgues S and Delavaux-Nicot B. J.Photochem. Photobiol.A:Chem. 2000; 132:137.
5.Hamciuc C, Hamciuc E and Bruma M.Polymer, 2005; 46: 5851
6.Ataei S M and Babanzadeh S. Appl. Organomet. Chem., 2007; 21: 360
7. Mansoori Y, Sarvari R, Zamanloo M R and Imanzadeh G H. Chinese J. Polym. Sci.,2010; 28: 21 4
8. Patil Y S, Mahindrakar J N, Salunkhe P H,Ubale V P and Ghanwat A A . J. Macromol.Sci. 2018 ; 55:572.
9. Oniwa K, Kikuchi H, Kanagasekaran T,Shimotani H, Ikeda S, Asao N,Yamamoto Y,Tanigaki K and Jin T. Chem. Commun.2016; 52, 4926–4929.
10.Zahradník P, Magdolen P and Zahradník P.Tetrahedron Lett. 2010 ;51, 5819.
11. Kuwabara J, Kuramochi M, Liu S,Yasuda T and Kanbara T. Polym. J. 2017; 49,123–131.
12.Tamami B and Yeganeh H.Polymer,2001;42:415.
13. Tamami B and Yeganeh H.Eur Polym J,2002;38:933.
14.Yamazaki N, Matsumoto M and Higashi F. J Polym Sci Polym Chem Ed 1975; 13:1373–1380.
15. Amininasab SM, Esmaili S and Shami Z. J Macromol Sci A 2020; 57: 35.
16. Aly KI, Khalaf AA and Alkskas IA. Eur Polym J. 2003; 39: 1035.
17. Aly KI, Khalaf AA and Alkskas IA. Eur Polym J. 2003; 39: 1030.
18. Alkskas IA and El-Gnidi BA. J Macromol Sci Chem. 2006; 25:345.
19. Vogel A. Textbook of Practical Organic Chemistry, Vol. 1. London: Longmans &Green ;1967. p. 646.
20.Tomlinson ML. J. Chem Soc. 1946;756.
21. Bauer AW, Kirby WMM, Sherris JC and Turck M. Am. J. Pathol, 1966; 49: 493.
22. Mikroyannidis J A. Eur Polym J.1989; 25:557.
23. Morgan PW. Condensation Polymers by Interfacial and Solution Methods. Interscience:New York, 1965; 5.
24. Negi YS, Suzuki YI, Kawamura I,Kakimoto MA and Imai Y. J.Polym. Sci. Polym. Chem. 1996; 34: 1663.
25. Varma IK, Kumar R and Bhattacharyya AB. J. Appl. Polym. Sci. 1990; 40: 531.
26. Yamashita M, Kakimoto MA and Imai Y. J. Polym. Sci. Polym. Chem. 1993; 31: 1513.
27. Aguilar-Vega M and Paul DR. J. Polym. Sci. Polym. Phys. Edn 1993;31: 1599.
28. Liou GS, Hsiao SH, Ishida M, Kakimoto M and Imai Y. J. Polym.Sci. Part A: Polym. Chem. 2002; 40: 2810.
29.Andrews RJ and Grulke EA. Glass transition temperatures of polymers. In Polymer Handbook, 4th edn, Bandrup J,Immergut EH, Grulke EA (eds). Wiley: New York, 1999;197.